Edge mapping
               Source:The SiteAuthor:admin Addtime:2021/6/23 Click:0
               
	
  
	
		
			
				Definition
			
			
				
					- 
						Edges showing through in the top coat.
					
 
	 
 
	
		
			
				Cause
			
			
				
					- 
						Old paintwork not sanded down smoothly at the edges. 
					
- 
						Putty and surfacer applied on top of elastic factory finish. 
					
- 
						Surfacer sanded and recoated before it had fully dried. 
					
- 
						Substrate not completely dry.
					
- 
						Priming material applied in excessive film thickness and not allowed to dry properly.
					
				Prevention
			
			
				
					- 
						Carry out a solvent test on the substrate (elastic / hard). 
					
- 
						Apply putty to bare metal only.
					
- 
						On elastic substrates apply surfacer to complete panels.
					
				Remedy
			
			
				
					- 
						After the top coat has fully dried, fine-sand and polish. 
					
- 
						Sand, isolate with a surfacer and spray again.